Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of a section cut transverse to the center of the body.  The crack is brittle, trough wall, and was arrested in the region where the valve body was welded to the insert.
105
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Transverse Section AspectDf - Cracking