Pipe

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center
ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Center

More from these cases

ML00065 — Erosion Corrosion of Monel PipingM - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Kalling Etched Micrography by OMDf - Weld Metal in the Center
ML00066 — GMAW Welded Joint in 9%Ni Alloy SteelM - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
ML00066 / May.2017
GMAW Welded Joint in 9%Ni Alloy Steel
M - Nickel Alloy SteelP - Welded Testpiece for QualificationAp - PipelineCd - Welding
Cm - Eletrolytically Etched Micrography by OMDf - Weld Metal in the Center