Crevice Corrosion in a Subsea System — Aspect Before Analysis

After a longitudinal cut of the case it was possible to see that a localized corrosion has occurred associated to the regions where there were sealed holes, plugged, in a crevice condition, not related to any welded position.
193
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Transverse Section AspectDf - Corrosion

More from these cases

ML00122 — Crevice Corrosion in a Subsea SystemM - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Macrography of the longitudinal section of the case, that was welded to padeyes. The corrosion occurred in a region where there were no microstructural changes, only the hole that was sealed with a plug and suffered a crevice corrosion mechanism.
145
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Corrosion
The macrography of a longitudinal section of the case shows one region where a through wall localized corrosion has occurred (in the left side of the image) and regions where the case was welded to a padeye, without any corrosion damage.
141
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Macro Oxalic Acid Electrolytic EtchedDf - Corrosion
ML00122 / Feb.2018
Crevice Corrosion in a Subsea System
M - Austenitic Stainless SteelP - CaseAp - Oil and GasCd - Crevice
Cm - Transverse Section AspectDf - Localized Corrosion