Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Brittle Cracks
More from these cases

ML00157 / Feb.2020
Bolts Under Chloride SCC Conditions
M - Austenitic Stainless SteelP - BoltAp - Oil and GasCd - Stress Corrosion
Cm - Surface Aspect by SEMDf - Brittle Fracture