Precipitation Hardened

3 cases · 18 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - At the Surface
Detail of the fracture surface, predominantly transgranular with secondary cracks of intergranular morphology.
831
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture

More from these cases

ML00145 — Impact of a .380 Winchester on 6061 T6 PlateM - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Elongated Dimples
ML00145 / Sep.2018
Impact of a .380 Winchester on 6061 T6 Plate
M - Aluminum Magnesium SiliconP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Ductile Fracture

+2 more from this case →

ML00137 — Brittle Fracture of a 15-5 PH Valve SpringM - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Intergranular Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Fracture
ML00137 / Mar.2021
Brittle Fracture of a 15-5 PH Valve Spring
M - Precipitation Hardened Stainless SteelP - SpringAp - Oil and GasCd - Brittle Behavior
Cm - Fractography by SEMDf - Transgranular Fracture

+2 more from this case →

ML00078 — Hydrogen Cracking of IN 718 Subsea ConnectorM - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
ML00078 / Jun.2017
Hydrogen Cracking of IN 718 Subsea Connector
M - NiCrFe AlloyP - ForgingAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Brittle Fracture