Acicular Ferrite

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The tube microstructure is ferritic-pearlitic, typical of this kind of material.  No evidences of microstrutural changes were detected (no overheating, no decarburization).
177
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by OMDf - Ferrite and Pearlite

More from these cases

ML00163 — Corrosion Fatigue of a Boiler Waterwall TubeM - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Nital Etched Micrography by SEMDf - Pearlite