Crevice Corrosion in a Subsea System — Aspect Before Analysis
Low Alloy Steel — sub-branches

ML00181 / Apr.2022
Wear of a Carburized Hypoid Gear
M - Low Alloy for Thermochemical TreatmentP - Pinion-crown assemblyAp - ShipCd - Wear
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00116 / Jan.2018
CMn Steel Structural Tubing 6 mm thick
M - CMn SteelP - Seamless Round ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00115 / Jan.2018
CMn Steel Structural Tubing 5 mm thick
M - CMn SteelP - Seamless Round ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00114 / Jan.2018
CMn Steel Structural Tubing 8 mm thick
M - CMn SteelP - Seamless Round ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness

ML00081 / Aug.2017
Hydrogen Cracking of a Chromium Plated Carburized Pin
M - Low Alloy for Thermochemical TreatmentP - Chromium PlatedAp - AutomotiveCd - Hydrogen Embrittlement
Cm - Nital Etched Micrography by OMDf - In the Center of the Thickness