CrMo Steel

2 cases · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Macrography of the welded joint between the forging and the pipe, showing it was welded in a narrow gap, indicating by the arrow the location of the crack at the margin of the weld, in the forging side.
129
ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - NItal Etched MacroDf - Welded Joint
Identification of the regions of metallographies of the base metal, heat affected zone (HAZ) and weld metal. Locations in the root, in the center of the thickness and close to the tube OD (external surface).
118
ML00177 / Dec.2021
Cr-Mo Seam Welded Tube
M - CrMo SteelP - Longitudinally Seam WeldedAp - Fired HeaterCd - Not according to spec
Cm - NItal Etched MacroDf - Welded Joint