Super Duplex Stainless Steel

7 cases · 36 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the longitudinal section, in the center of the thickness of the pin, presenting an aligned ferritic-austeinitic structure.
180
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
Microstructural analysis of the valve body structure, close to the position where the cracking has occurred.  The structure is ferritic austenitic, with a large amount of detrimental phases associated to the ferritic structure, probably sigma phase.
106
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - NaOH Electrolytic Etched MicroDf - Sigma
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrography of the flange in the longitudinal section. The flange microstructure is ferritic austenitic, presenting a coarse structure.
102
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure

More from these cases

ML00146 — Plastic Deformation of a SDSS Riser PinM - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Micrography of a longitudinal section, at the surface of the pin, where the thermal spray layer is sound. The thickness of the layer is about 0.3 mm.
168
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
Micrographic detail of a longitudinal section of the pin, at the surface, evidencing the thermal spray layer, about 0.3 mm.  The layer presents typical characteristics of multiple layers, low amount of entrapped oxides and pores.  The interface presents a high roughness level for a good adherence and some entrapped oxides. The structure of the SDSS substrate did not show thermal effects.
154
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
ML00134 — Brittle Fracture of a Superduplex Valve BodyM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Micrographic detail of the valve body structure, close to the position where the cracking has occurred.  The structure is ferritic austenitic, with a large amount of detrimental phases associated to the ferritic structure, probably sigma phase.
102
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - NaOH Electrolytic Etched MicroDf - Sigma
Metallographic detail of the large amount of sigma phase, associated to the ferritic structure.
105
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - NaOH Electrolytic Etched MicroDf - Sigma
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Micrography by SEMDf - Sigma
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Micrography by SEMDf - Sigma
ML00134 / Aug.2020
Brittle Fracture of a Superduplex Valve Body
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Fracture
Cm - Micrography by SEMDf - Sigma

+4 more from this case →

ML00123 — Non Qualified Superduplex for SubseaM - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
ML00123 / Feb.2018
Non Qualified Superduplex for Subsea
M - Super Duplex Stainless SteelP - BarAp - Oil and GasCd - Not according to spec
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
ML00100 — Superduplex Tubing to Forging Welded JointM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 — MIC of a Subsea Hydraulic LineM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Grain refined structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Strain Hardened
ML00049 — Pipe to Flange Welded Joint in a 14" ND Superduplex SpoolM - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - Electrolytic Etch Micrography by SEMDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - Electrolytic Etch Micrography by SEMDf - Duplex structure

+2 more from this case →

ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
113
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
100
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - Electrolytic Etch Micrography by SEMDf - Delta ferrite