Martensitic Stainless Steel
4 cases · 7 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Martensite

ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Kalling Etched Micrography by SEMDf - Martensite
More from these cases

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite

ML00092 / Sep.2017
MIC of a Valve Body
M - Martensitic Stainless SteelP - Valve BodyAp - Oil and GasCd - Brittle Behavior
Cm - Kalling etched, OMDf - Martensite

ML00054 / Dec.2018
Cutlery Corrosion
M - Martensitic Stainless SteelP - Foodstuff ArticleAp - KitchenCd - Pitting Corrosion
Cm - Kalling Etched Micrography by SEMDf - Martensite