Martensitic Stainless Steel

4 cases · 6 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00148 / Sep.2018
Brittle Fracture of a 420 SS Barrel Nut
M - Martensitic Stainless SteelP - Barrel NutAp - LiftingCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00039 / Apr.2017
Collapse in Tubular 13Cr
M - Martensitic Stainless SteelP - Seamless PipeAp - Oil and GasCd - Heat Treatment Defect
Cm - Kalling Etched Micrography by OMDf - Martensite

More from these cases

ML00124 — MIC of a Martensitic Valve RingM - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
ML00124 / Feb.2018
MIC of a Martensitic Valve Ring
M - Martensitic Stainless SteelP - ForgingAp - EnergyCd - Brittle Behavior
Cm - Kalling Etched Micrography by OMDf - Martensite
ML00085 — Corrosion Fatigue of a Martensitic SS PinM - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite