Low Carbon Steel

2 cases · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the tube internal surface after removal from the boiler, presenting multiple longitudinal cracks.
295
ML00163 / Jun.2020
Corrosion Fatigue of a Boiler Waterwall Tube
M - Low Carbon SteelP - Seamless tubeAp - BoilerCd - Corrosion Fatigue
Cm - Aspect Before AnalysisDf - Internal Surface
ML00140 / May.2019
Preferential Corrosion of Pipe Seam Weld
M - Low Carbon SteelP - Longitudinal Seam Welded PipeAp - ShipCd - Preferential Dissolution
Cm - Aspect Before AnalysisDf - Internal Surface