Crevice Corrosion in a Subsea System — Aspect Before Analysis

The fracture micromechanism is ductile for the pin that has been sheared in a condition of controlling the load carrying. Elongated Dimples.
453
ML00007 / Dec.2020
Free Machining Brass in Shear Pin
M - BrassP - Machined PartAp - LiftingCd - Shear
Cm - Fractography by SEMDf - Elongated Dimples