Crevice Corrosion in a Subsea System — Aspect Before Analysis

Cast Iron — sub-branches

Micrography of a crankshaft longitudinal section at the shaft edge, in the as polished condition, presenting nodular graphite, well distruibuted.
139
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - At the Surface
The cast iron microstructure is predominatly ferritic with graphite nodules.
169
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
Grey cast iron microstructe. Perlitic matrix and graphite flakes.
508
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Pearlite Matrix
Polished cross-section showing rounded graphite nodules within a ferritic matrix, bordered by an irregular oxidized region at the surface edge.
910
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Oxide Layer

More from these cases

ML00154 — High Strength Cast Iron CrankshaftM - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
As polished micrography of the crankshaft at the shaft edge, close to the surface.  Graphite in nodules.
126
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
As polished micrographic detail of the graphite in nodules, close to the surface of the shaft edge, in a longitudinal section.
114
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - As polished micrographyDf - Graphite in Nodules
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - At the Surface
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite
ML00154 / Jan.2019
High Strength Cast Iron Crankshaft
M - Nodular Cast IronP - CastingAp - EngineCd - Surface treatment
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite

+12 more from this case →

ML00040 — Brittle Fracture of a Valve StemM - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
The micrography of the stem at the fracture region shows a flat fracture with transgranular clevage at the ferritic structure.
137
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture
Micrography presenting a detail of the fracture surface opening to the graphite nodules.
139
ML00040 / Apr.2017
Brittle Fracture of a Valve Stem
M - Nodular Cast IronP - Valve StemAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Fracture
ML00032 — Cast Iron Case of Drilling EquipmentM - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Low magnification micrography presenting the grapjite morphology.
138
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Micrography by OMDf - Graphite Type A (ASTM A247)
Grey cast iron structure.  As polished.
111
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Micrography by OMDf - Graphite in Flakes
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Micrography by OMDf - Graphite in Flakes
Grey cast iron with graphite in flakes and perlitic matrix.
110
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Perlite Matrix
ML00032 / Jan.2017
Cast Iron Case of Drilling Equipment
M - Gray Cast ironP - CastAp - O&G Well DrillingCd - Typical manufacturing
Cm - Nital Etched Micrography by OMDf - Graphite Type A (ASTM A247)

+1 more from this case →

ML00001 — Thermal Fatigue of Cast IronM - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
The 1" flat casting product presents a ferritic perlitic matrix and graphite nodules.
112
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Graphite in Nodules
Center of the flat casting product, presenting nodular graphite and ferritic perlitic matrix.
113
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Predominantly Ferritic Matrix
Nodular cast iron presenting a ferritic perlitic matrix.
109
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Matrix of ferrite and pearlite
Nodular cast iron.  Ferritic perlitic matrix. White regions in the pearlite colonies are free carbides.
129
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Free Carbides in Pearlite Colonies
The graphite nodules remain at the surface and the matrix was consumed during high temperature exposition.
117
ML00001 / Dec.2017
Thermal Fatigue of Cast Iron
M - Nodular Cast IronP - CastAp - SiderurgyCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Oxide Layer