Welding Defect

3 cases · 8 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Welding Defect — sub-branches

ML00173 / May.2021
Welding Cracks in an Aged HP Cast Fitting
M - Heat Resistant SteelP - Cast FtittingAp - PetrochemicalCd - Welding
Cm - Kalling Etched Micrography by OMDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Lack of fusion

More from these cases

ML00162 — Valve Body Crack Growth from Weld DefectsM - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - Nital Etched Micrography by OMDf - Hot cracking
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M - Low Alloy Medium Carbon QTP - Valve BodyAp - O&G Well DrillingCd - Fatigue Induced by a Defect
Cm - As polished micrographyDf - Hot cracking
ML00150 — Vibration Induced Fatigue in a SS Oil PipingM - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Lack of fusion