Hot cracking
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Detail focus
/
Welding Defect
/ Hot cracking
Capture method: Nital Etched Micrography by OM
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
28
VIEW
ML00162 / Apr.2020
Valve Body Crack Growth from Weld Defects
M
- Low Alloy Medium Carbon QT
P
- Valve Body
Ap
- O&G Well Drilling
Cd
- Fatigue Induced by a Defect
Cm
- Nital Etched Micrography by OM
Df
- Hot cracking