Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrography of the longitudinal section, in the center of the thickness of the pin, presenting an aligned ferritic-austeinitic structure.
180
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Ferrite and Austenite
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrography of the flange in the longitudinal section. The flange microstructure is ferritic austenitic, presenting a coarse structure.
102
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure

More from these cases

ML00146 — Plastic Deformation of a SDSS Riser PinM - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Micrography of a longitudinal section, at the surface of the pin, where the thermal spray layer is sound. The thickness of the layer is about 0.3 mm.
168
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
Micrographic detail of a longitudinal section of the pin, at the surface, evidencing the thermal spray layer, about 0.3 mm.  The layer presents typical characteristics of multiple layers, low amount of entrapped oxides and pores.  The interface presents a high roughness level for a good adherence and some entrapped oxides. The structure of the SDSS substrate did not show thermal effects.
154
ML00146 / Jul.2018
Plastic Deformation of a SDSS Riser Pin
M - Super Duplex Stainless SteelP - PinAp - O&G Well DrillingCd - Bending
Cm - NaOH Electrolytic Etched MicroDf - Coating Layer
ML00100 — Superduplex Tubing to Forging Welded JointM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00100 / Nov.2017
Superduplex Tubing to Forging Welded Joint
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Welding
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 — MIC of a Subsea Hydraulic LineM - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Grain refined structure
ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Strain Hardened
ML00049 — Pipe to Flange Welded Joint in a 14" ND Superduplex SpoolM - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Fusion Line
ML00049 / Apr.2017
Pipe to Flange Welded Joint in a 14" ND Superduplex Spool
M - Super Duplex Stainless SteelP - Piping spoolAp - Oil and GasCd - Removed From Service
Cm - NaOH Electrolytic Etched MicroDf - Fusion Line
ML00002 — Preferential Dissolution and Cracks in SDSSM - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
113
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Duplex structure
Micrographic detail of the flange microstructure in the longitudinal section. The flange is ferritic austenitic, presenting 70% of austenite. In the ferrite network there are evidences of precipitation/formation of detrimental phases.
100
ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution