Microstructure

2 cases · 5 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The microstructure of the pipe base metal, in the center of the thickness, is granular alpha.
102
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Granular structure
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
114
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite

More from these cases

ML00005 — Environmental Hydrogen Damage in Ti PipeM - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
ML00005 / Apr.2017
Environmental Hydrogen Damage in Ti Pipe
M - Unalloyed TitaniumP - Longitudinal Seam Welded PipeAp - PipingCd - Hydride Formation
Cm - Kroll Etched Micrography by OMDf - Columnar Grains
ML00011 — Intergranular SCC of Pure NickelM - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Microstructure of the fitting in the transverse section, presenting a granular Ni austenitic structure.  No evidences of any phase in the grain boundaries.
110
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite
ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Kalling Etched Micrography by OMDf - Austenite