Non Metallic Inclusions
3 cases · 4 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00035 / Dec.2017
Carbon Steel L Shape
M - Low Carbon SteelP - Rolled ShapeAp - StructureCd - Removed From Service
Cm - Nital Etched Micrography by OMDf - Non Metallic Inclusions

ML00103 / Nov.2017
Brittle Fracture of a Free-Cutting Connector
M - Low Carbon SteelP - Machined PartAp - ShipCd - Brittle Fracture
Cm - Nital Etched Micrography by OMDf - Non Metallic Inclusions

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Micrography by OMDf - Non Metallic Inclusions
More from these cases

ML00017 / Apr.2017
Casting Defect in CA6NM
M - Martensitic Stainless SteelP - Machined PartAp - EnergyCd - Casting Defect
Cm - Kalling Etched Micrography by OMDf - Non Metallic Inclusions