Martensite

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Micrographic detail of the rolled thread that was heat treated later. The bolt was quenched and tempered to 30 HRc and presented a martensitic structure.
110
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Nital Etched Micrography by OMDf - Martensite

More from these cases

ML00130 — Fatigue Fracture of Overloaded BoltsM - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
The microstructure of the bolt is martensitic in the center of the thickness. Longitudinal section.
103
ML00130 / Jun.2018
Fatigue Fracture of Overloaded Bolts
M - Low Alloy Medium Carbon QTP - FastenerAp - O&G Well DrillingCd - Mechanical Fatigue
Cm - Nital Etched Micrography by OMDf - Martensite