Coarse Structure
3 cases · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Damage ×Microstructure: Duplex Ferritic Austenitic ×Capture method: Optical Microscope ×clear all

ML00150 / Dec.2018
Vibration Induced Fatigue in a SS Oil Piping
M - Duplex Stainless SteelP - PipingAp - FPSOCd - Vibration Induced Fatigue
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure

ML00094 / Sep.2017
MIC of a Subsea Hydraulic Line
M - Super Duplex Stainless SteelP - Fabrication WeldAp - SubseaCd - Brittle Behavior
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure

ML00002 / Jan.2018
Preferential Dissolution and Cracks in SDSS
M - Super Duplex Stainless SteelP - Fabrication WeldAp - PipingCd - Preferential Dissolution
Cm - NaOH Electrolytic Etched MicroDf - Coarse Structure