Bainite

2 cases · 4 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Bainite
ML00108 / Dec.2017
Thermal Spray Layer in a Pinion Shaft
M - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
Cm - Nital Etched Micrography by OMDf - Bainite

More from these cases

ML00109 — Thermal Spray and Fuse Layer in Forged PinM - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Bainite
ML00108 — Thermal Spray Layer in a Pinion ShaftM - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
ML00108 / Dec.2017
Thermal Spray Layer in a Pinion Shaft
M - High Strength Low AlloyP - ShaftAp - EngineCd - Coating Defect
Cm - Nital Etched Micrography by OMDf - Bainite