Bainite

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The thick wall tube presented a bainitic structure at the surface, where the replica was conducted. The base material material hardness is 167 HB.
108
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Nital etched, OMDf - Bainite