Martensite
2 cases · 4 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Martensite

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite
More from these cases

ML00109 / Jan.2018
Thermal Spray and Fuse Layer in Forged Pin
M - Low Alloy Medium Carbon QTP - Tubular ForgingAp - O&G Well DrillingCd - Thermal spray
Cm - Nital Etched Micrography by OMDf - Martensite

ML00085 / Nov.2017
Corrosion Fatigue of a Martensitic SS Pin
M - Martensitic Stainless SteelP - Forged PinAp - O&G Well DrillingCd - Corrosion Fatigue
Cm - Kalling Etched Micrography by OMDf - Martensite