VIEW
ML00088 / Dec.2017
Hydrogen Cracking of an API 5D S135 Drill Pipe
M
- Low Alloy Medium Carbon QT
P
- Drill Pipe
Ap
- Subsea
Cd
- Hydrogen Embrittlement
Cm
- Surface Aspect by SEM
Df
- Intergranular Cracking