Intergranular Cracking
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Condition: Stress Corrosion ×Microstructure: Austenite ×Capture method: Optical Microscope ×clear all

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Micrography by OMDf - Intergranular Cracking
More from these cases

ML00011 / Oct.2017
Intergranular SCC of Pure Nickel
M - Unalloyed NickelP - Wrought FittingAp - Chemical IndustryCd - Stress Corrosion
Cm - Micrography by OMDf - Intergranular Cracking