Intergranular Cracking
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M - Aluminum BronzeP - Seamless tubeAp - Oil and GasCd - Stress Corrosion
Cm - FeCl3+HCl+H2O Etched MicroDf - Intergranular Cracking