Ductile Behavior of an Aluminum Wheel
M - Aluminum Silicon MagnesiumP - CastingAp - AutomotiveCd - Ductile Behavior
Cm - Keller Etched MacroDf - Fracture
The macrography of the welded joint shows the AA 6063 alloy pipe in the right and the AA 3003 pipe in the left, welded in two passes.  The root presents small regions of corrosion in the weld metal and a localized corrosion at the fusion line of the 6063 pipe (knife-line attack morphology).
397
ML00059 / Feb.2018
Intergranular Corrosion of Aluminum Piping
M - Aluminum ManganeseP - Welded JointAp - Chemical IndustryCd - Intergranular Corrosion
Cm - Keller Etched MacroDf - Localized Corrosion