Damage

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Acetate metallographic replica from the surface, before cracking removal, showing the intergranular morphology of the cracks in a very refined weld metal structure.
123
ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital etched, OMDf - Intergranular Cracking

More from these cases

ML00010 — Cold Cracks in a Gouged Weld MetalM - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Detail of the acetate metallographic replica from the surface, before cracking removal, showing the (previous austenite) intergranular morphology of the cracks in a very refined weld metal structure.
107
ML00010 / Oct.2017
Cold Cracks in a Gouged Weld Metal
M - Low Alloy Low Carbon QTP - Rolled PlateAp - OffshoreCd - Welding Defect
Cm - Nital etched, OMDf - Intergranular Cracking