Damage

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Aspect of the heat exchanger plate showing the rupture of the plate in multiple cracks, starting at the side of the crude oil with high salinity.
727
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking