Damage

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Transverse section of the 2" diameter pipe at the pitting location.  The pipe was leaking.
1323
ML00014 / Apr.2017
Pitting Corrosion in 316SS Pipe
M - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Cm - Transverse Section AspectDf - Pitting