Crevice Corrosion in a Subsea System — Aspect Before Analysis

Damage — sub-branches

Aspect of the heat exchanger plate showing the rupture of the plate in multiple cracks, starting at the side of the crude oil with high salinity.
727
ML00051 / Apr.2020
Chloride SCC of 316 Heat Exchanger Plate
M - Austenitic Stainless SteelP - Heat Exchanger PartAp - FPSOCd - Stress Corrosion
Cm - Aspect Before AnalysisDf - Cracking
The external surface of the 2" diameter pipe is rusted and the leakage is associated to “holes” that appear very small at the surface but that open a large hole in the middle of the thickness.
507
ML00014 / Apr.2017
Pitting Corrosion in 316SS Pipe
M - Austenitic Stainless SteelP - Seamless PipeAp - FPSOCd - Pitting Corrosion
Cm - Aspect Before AnalysisDf - Corrosion