Transgranular Cracking

2 cases · 6 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00119 / Feb.2018
Thermal Fatigue of a Marine Boiler
M - Low Carbon SteelP - Fabrication WeldAp - ShipCd - Thermal Fatigue
Cm - Nital Etched Micrography by OMDf - Transgranular Cracking
Micrography of a transverse section of the shell plate in a cracked position showing the transgranular morphology of the stress corrosion cracks.
167
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Cracking

More from these cases

ML00019 — Transgranular SCC in Boiler Steam DrumM - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
Micrographic detail of the transgranular stress corrosion cracking.
157
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by OMDf - Transgranular Crack
ML00019 / Apr.2017
Transgranular SCC in Boiler Steam Drum
M - CMn SteelP - Rolled PlateAp - BoilerCd - Stress Corrosion
Cm - Nital Etched Micrography by SEMDf - Transgranular Crack