ML00168 / Aug.2020
SCC of Austenitic SS Flange Stub End
M
- Austenitic Stainless Steel
P
- Stub End
Ap
- Chemical Industry
Cd
- Stress Corrosion
Cm
- As polished micrography
Df
- Multiple cracks