Leakage

2 cases · 2 images for “corrosion”

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Detail of the transverse section of the 4" pipe at the longitudinal seam weld evidencing the leakage position.  The damage appears as a through wall opening.  The pipe thickness is 8 mm and there are no evidences of general corrosion (the SCH 80 corresponds to 8.6 mm) or pitting at the internal surface.
100
ML00140 / May.2019
Preferential Corrosion of Pipe Seam Weld
M - Low Carbon SteelP - Longitudinal Seam Welded PipeAp - ShipCd - Preferential Dissolution
Cm - Transverse Section AspectDf - Leakage
Detail of the internal piping surface, showing lack of deposits and a shinning surface, suggesting erosive conditions.
226
ML00065 / May.2017
Erosion Corrosion of Monel Piping
M - NiCu AlloyP - Seamless PipeAp - Chemical IndustryCd - Erosion Corrosion
Cm - Surface AspectDf - Leakage