Intergranular Cracking
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Detail focus
/
Damage
/ Intergranular Cracking
Condition: Stress Corrosion
×
Microstructure: Alpha
×
Standard: C60800
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
113
VIEW
ML00165 / Jul.2020
SCC of Aluminum Bronze Heating Coil
M
- Aluminum Bronze
P
- Seamless tube
Ap
- Oil and Gas
Cd
- Stress Corrosion
Cm
- FeCl3+HCl+H2O Etched Micro
Df
- Intergranular Cracking