Intergranular Cracking

2 cases · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking
Fractographic aspect of the broken fastener, at the surface, showing na intergranular morphology typical of a hydrogen assisted mechanism of a high strenght steel under cathodic protection.
224
ML00074 / Jun.2018
Hydrogen Cracking of a 17-4 PH Subsea Bolt
M - Precipitation Hardened Stainless SteelP - FastenerAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking

More from these cases

ML00009 — Hydrogen Cracking of a 5" Drill Pipe S135M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
ML00009 / Sep.2017
Hydrogen Cracking of a 5" Drill Pipe S135
M - Low Alloy Medium Carbon QTP - Drill PipeAp - SubseaCd - Hydrogen Embrittlement
Cm - Fractography by SEMDf - Intergranular Cracking