Dimples
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Application: Structure ×Microstructure: Deformed Structure ×Capture method: Fractography by SEM ×clear all

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples
More from these cases

ML00143 / Aug.2018
Impact of a .308 Winchester on A36 Plate
M - Low Carbon SteelP - Rolled PlateAp - StructureCd - Pierced
Cm - Fractography by SEMDf - Dimples