Cracks

1 case · 3 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Aspect of the welded region after dye check showing several indications, later identified as hot cracks associated to the repair welding.
114
ML00070 / Jan.2019
Automotive Light Alloy Wheel Repaired By Welding
M - Aluminum Silicon MagnesiumP - RimAp - AutomotiveCd - Removed From Service
Cm - Aspect by NDTDf - Cracks

More from these cases

ML00070 — Automotive Light Alloy Wheel Repaired By WeldingM - Aluminum Silicon MagnesiumP - RimAp - AutomotiveCd - Removed From Service
ML00070 / Jan.2019
Automotive Light Alloy Wheel Repaired By Welding
M - Aluminum Silicon MagnesiumP - RimAp - AutomotiveCd - Removed From Service
Cm - Micrography by SEMDf - Cracks
ML00070 / Jan.2019
Automotive Light Alloy Wheel Repaired By Welding
M - Aluminum Silicon MagnesiumP - RimAp - AutomotiveCd - Removed From Service
Cm - Micrography by SEMDf - Cracks