Welding Defect
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Condition
/
Damage
/
Fabrication Defect
/ Welding Defect
Product: Fabrication Weld
×
Microstructure: Ferritic
×
Detail focus: Microstructure
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
51
VIEW
ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M
- CMn Steel
P
- Fabrication Weld
Ap
- Automotive
Cd
- Welding Defect
Cm
- Nital Etched Micrography by OM
Df
- Martensite