Welding Defect
2 cases · 3 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Standard: ASTM ×Capture method: Scanning Electron Microscope ×Detail focus: Heat Affected Zone ×clear all

ML00178 / Jan.2022
Cold cracks in Cr-Mo Welded Forging
M - CrMo SteelP - ForgingAp - O&G Well DrillingCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Heat Affected Zone

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Nital Etched Micrography by SEMDf - Heat Affected Zone
More from these cases

ML00052 / Apr.2017
Cold Cracks in API 5CT L80 Tube Welded to a Structural Part
M - Low Alloy SteelP - Seamless tubeAp - OffshoreCd - Welding Defect
Cm - Surface Aspect by SEMDf - Heat Affected Zone