Welding Defect
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Bainite ×Capture method: Optical Microscope ×Detail focus: Intergranular Cracking ×clear all

ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Intergranular Cracking
More from these cases

ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Intergranular Cracking