Welding Defect
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Atlas
/
Condition
/
Damage
/
Fabrication Defect
/ Welding Defect
Application: Mooring Chain
×
Microstructure: Bainite
×
Detail focus: Banded Structure
×
clear all
Results
Sort
Newest
Oldest
Title A-Z
Title Z-A
79
VIEW
ML00013 / Apr.2017
Welding Cracks in Mooring Chain
M
- Low Alloy Low Carbon QT
P
- Welded Part
Ap
- Offshore
Cd
- Welding Defect
Cm
- Nital Etched Micrography by OM
Df
- Banded Structure