Welding Defect

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Intergranular Cracking