Welding Defect

1 case · 1 image

Crevice Corrosion in a Subsea System — Aspect Before Analysis

Fracture occurred during fabrication of a low carbon steel automotive part, welded by SAW process in one fillet, between a superior plate (8mm thick) and an inferior plate (12 mm thick). See the schematic drawing in the next figure.
290
ML00069 / May.2017
Liquation Cracks in SAW of Low Carbon Steel
M - Low Carbon SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Aspect Before AnalysisDf - Fracture