Crevice Corrosion in a Subsea System — Aspect Before Analysis

The shaft was removed from service without a failure. It was 4' long and the diameters varied from 2 1/2" to 4 1/2". It was analyzed to be specified for purchasing a new one but properties evidenced bad ductility and brittle behavior even at ambient temperature, associated to a microestruture "as hot rolled".
1238
ML00152 / Dec.2018
Low Alloy Steel Pump Shaft
M - High Strength Low AlloyP - ShaftAp - Oil and GasCd - Removed From Service
Cm - Aspect Before AnalysisDf - General View
The shaft presented a light wear at the end of the life. See the schematic drawing in the next figure
598
ML00064 / Apr.2017
SAE 1045 Steel Shaft
M - Medium Carbon SteelP - ShaftAp - Mechanical IndustryCd - Removed From Service
Cm - Aspect Before AnalysisDf - At the Surface