Carburization
2 cases · 9 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Oxalic Acid Electrolytic EtchDf - Austenite

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Carburized Layer
More from these cases

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Oxalic Acid Electrolytic EtchDf - Ferrite and Austenite

ML00174 / Jul.2021
Carburization of a 347 SS Welded Joint
M - Austenitic Stainless SteelP - Fabrication WeldAp - EnergyCd - Carburization
Cm - Oxalic Acid Electrolytic EtchDf - Coarse Structure

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Bainite

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Bainite

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Bainite

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Bainite

ML00107 / Dec.2017
Carburized 9Cr1MoV Superheater Tube
M - Heat Resistant SteelP - Seamless tubeAp - BoilerCd - Carburization
Cm - Nital Etched Micrography by OMDf - Carburized Layer