Welding Defect

1 case · 2 images

Crevice Corrosion in a Subsea System — Aspect Before Analysis

The morphology of the cracking in the weld metal is intergranular (in the previous austenite grain boundaries), and branched. The replication technique was adopted to define the nature of the cracks.
148
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Nital etched, OMDf - Cracks

More from these cases

ML00071 — Reheating Cracking of a CrMo Vessel WeldM - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Detail of the weld metal intergranular and branched cracking (in the previous austenite grain boundaries). The replication technique was adopted to define the nature of the cracks.
125
ML00071 / Jan.2019
Reheating Cracking of a CrMo Vessel Weld
M - CrMo SteelP - In Field WeldAp - EnergyCd - Welding Defect
Cm - Nital etched, OMDf - Cracks