Welding Defect
1 case · 2 images
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Refined ferritic ×Capture method: Optical Microscope ×Detail focus: Base Metal ×clear all

ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Base Metal
More from these cases

ML00067 / May.2017
Cold Cracks in C-Mn SAW Weld Metal
M - CMn SteelP - Fabrication WeldAp - AutomotiveCd - Welding Defect
Cm - Nital Etched Micrography by OMDf - Base Metal