Damage
1 case · 1 image
Crevice Corrosion in a Subsea System — Aspect Before Analysis
Microstructure: Monophasic ×Capture method: Surface Aspect ×Detail focus: Sampling and Analysis ×clear all
Damage — sub-branches

ML00170 / Sep.2020
MIC in Aluminum Brass Tubes
M - Aluminum BrassP - Seamless tubeAp - MaritimeCd - Preferential Dissolution
Cm - Surface AspectDf - Internal Surface